Cutting Tools
The cutting edge is the smallest part of a machine tool, but it determines almost everything: how fast the machine operates, the quality of the finished surface, and the cost of each workpiece. In this chapter, we’ll look at tools as items to be selected: what materials they’re made of, how to read the codes for inserts and tool holders, what types of end mills, drill bits, and taps are available, and how to mount them on the machine. The physics of chip formation and wear is covered in Chapter 24; here, we’ll learn how to select tools and read a catalog.
25.1 What Is Required of a Cutting Material
A cutting edge operates under extremely harsh conditions: chip flows over it at hundreds of meters per minute, the tip reaches 800 or 1,000 °C, the pressure at the contact zone exceeds 1,000 N/mm², and, if the cut is interrupted, a shock is delivered with every revolution. To withstand these conditions, three qualities are required—though they are mutually exclusive:
- heat resistance: the cutting edge must remain harder than the workpiece even when it is red-hot; ordinary steel softens at 600 °C, but carbide does not;
- wear resistance: abrasion, adhesion, diffusion, and oxidation wear down the cutting edge (the mechanisms are explained in Chapter 24); the harder and more chemically stable the material, the longer it lasts;
- Toughness: the ability to absorb impacts and vibrations without chipping; it is useful in roughing, on castings, during interrupted cuts, and on machines with low rigidity.
A very hard material is usually brittle, while a very tough material is usually ductile. For this reason, there is no such thing as the perfect cutting material: each material falls into a specific zone on the diagram in Figure 25.1, and you choose the one that works best for the job. The higher up the diagram you go, the higher the cutting speed can be; the further to the right you go, the better the tool withstands impacts and unpredictable conditions.
In addition to these three qualities, other factors include chemical stability (diamond, for example, reacts with iron when heated and cannot be used on steel), thermal conductivity, the ability to sharpen a cutting edge, and, of course, price. In the following paragraphs, we’ll look at each family one by one, from the most tenacious to the hardest.
25.2 High-Speed Steels: HSS, HSS-Co, and Powdered Metal Steels
The high-speed steels (HSS, high-speed steel) are alloy steels containing high levels of tungsten, molybdenum, vanadium, and chromium, which are quenched and tempered several times to a hardness of 62–66 HRC. The hard carbides dispersed throughout the matrix provide wear resistance, and secondary tempering (Chapter 22) ensures that the hardness remains high up to approximately 550–600 °C. Above this temperature, the cutting edge softens abruptly; for this reason, HSS operates at cutting speeds 5 to 8 times lower than those of cemented carbide.
Its main strength is its toughness: an HSS tool can be sharpened to a very fine edge, withstands bending and vibration, and is inexpensive. It is still widely used for drill bits, taps, reamers, form cutters, broaches, and hobbing cutters, as well as for homemade specialty tools and on older or less rigid machines.
- HSS (for example, HS6-5-2, the classic M2): the numbers represent the percentages of tungsten, molybdenum, and vanadium; it is the most common;
- HSS-Co (HS6-5-2-5, HS2-9-1-8): containing 5–8% cobalt, harder when hot; suitable for stainless steel, alloy steels, and hard cast iron, though slightly less tough;
- Powder-metal HSS (HSS-PM): The atomized and hot-pressed powder produces extremely fine, uniformly distributed carbides; it is possible to incorporate more alloy and more carbides without sacrificing toughness, up to 67–70 HRC. It is the material of choice for high-quality HSS taps and end mills, which are often coated.
| Type | Hardness (HRC) | Works up to about (°C) | Vc on C45 steel (m/min) |
|---|---|---|---|
| HSS (HS6-5-2) | 62-65 | 550 | 25-35 |
| HSS-Co (HS6-5-2-5) | 64-67 | 600 | 30-40 |
| Powder-coated HSS | 65-70 | 600 | 35-50 |
These are approximate, rounded values prepared by CNC Simulator Italia for comparison purposes. Actual speeds depend on the tool (drill bit, end mill, tap) and should be taken from the catalog.
25.3 Hard Metal
The hard metal (in English cemented carbide, often called “Widia” in the workshop—named after an old brand—is not a cast metal but a material sintered: powder of tungsten carbide Toilet mixed with powder of cobalt Cobalt, pressed into the shape of the insert and heated to approximately 1400–1500 °C. The cobalt melts, coats the carbide grains, and, as it cools, holds them together just as cement holds gravel in concrete. During sintering, the workpiece shrinks by about 18% in every direction; for this reason, inserts “as they come out of the furnace” have wider tolerances than ground ones.
The properties are adjusted using two “knobs”:
- the amount of cobalt, usually between 5 and 12 percent: more cobalt means greater toughness and less hardness;
- The grain size of WC: from more than 3 µm (coarse grain, tough) to less than 1 µm (micrograin, very hard and capable of maintaining a sharp edge). Solid-carbide end mills and drill bits almost always use micrograin with 8–12% cobalt.
To machine steel, cubic carbides of titanium, tantalum, and niobium (TiC, TaC, NbC) are also added: they offer better resistance to diffusion—that is, to the hot iron in the chip that “melts” the tungsten carbide and carves a crater into the face of the insert. Many modern inserts also have a cobalt-enriched surface layer about twenty micrometers thick: the core remains hard and resistant to deformation, while the outer layer is more ductile and helps prevent cracks from forming at the cutting edges.
Cemented carbide has a hardness ranging from 1,300 to 1,800 HV, remains hard up to about 900–1,000 °C, and is about three times stiffer than steel (module of elasticity around 600,000 N/mm² versus 210,000): this is important for boring bars and long milling cutters (section 25.9). The downside is brittleness: an insert that strikes an edge or vibrates will chip, whereas an HSS insert would simply bend.
25.4 ISO 513 Classes: Groups P, M, K, N, S, H
There are hundreds of grades of cemented carbide, and each manufacturer gives them a trade name. To help navigate this, the ISO 513 standard is used, which divides the materials to be machined into six groups, each identified by a letter and a color, and within each group, indicates the application range with a number:
- low number (01, 05, 10): harder, more wear-resistant grade, for finishing operations, continuous cutting, high speeds, and low feeds;
- High number (30, 40, 50): tougher grade, for roughing, interrupted cuts, scale, low speeds, and less stable machines;
- The middle values (15, 20, 25) are the “universal” grades, which are the best-selling ones.
| Group | Color | Materials | What makes them difficult |
|---|---|---|---|
| P 01-50 | blue | unalloyed and alloyed steels, cast steel, ferritic and martensitic stainless steels | long chips, crater wear due to diffusion |
| M 01-40 | yellow | austenitic and duplex stainless steels | work hardening, tough chips, heat, built-up cutting edge |
| K 01-40 | red | gray, spheroidal, and malleable cast iron | short but abrasive chips, casting scale |
| N 01-30 | green | aluminum, copper, brass, plastics, composites | Material buildup on the cutting edge, abrasion (Al-Si, fibers) |
| S 01-30 | brown | nickel-cobalt superalloys, titanium | heat retention on the cutting edge, high heat resistance |
| H 01-30 | gray | hardened steels (45–65 HRC), shell cast iron | hardness of the workpiece, extremely high pressures on the drill bit |
On insert boxes and in catalogs, the grade is indicated by colors and a range, for example, “P15-P30, M20.” The same insert may cover multiple groups: many coated grades for steel are also suitable for cast iron. The same groups are used for cutting parameter tables, such as the one in section 26.12.
25.5 Cermets, Ceramics, CBN, and PCD
Cermet
The name comes from “ceramic plus metal”: these are sintered materials like cemented carbide, but the hard grains are made of titanium carbonitride (TiCN) instead of tungsten carbide, bonded with nickel and cobalt. They have lower affinity for iron and produce polished surfaces even without a coating; they are used for finishing steel at high speeds and low feeds, with light passes. They are less tough than cemented carbide and are susceptible to thermal shock: they should be machined dry or with abundant, constant coolant, never with intermittent jets.
Ceramics
- Al₂O₃-based ceramics, either pure (white) or mixed with titanium carbide (black): extremely hard and highly stable at high temperatures, for the rapid finishing of gray cast iron and hardened steels, for continuous cutting only;
- silicon nitride Si₃N₄ (and SiAlON): more durable, resistant to thermal shock; these are the ceramics used for roughing of gray cast iron and nickel superalloys;
- Whisker-reinforced ceramics: Al₂O₃ with crystalline silicon carbide fibers that halt crack propagation; for nickel superalloys, at speeds 5 to 10 times those of cemented carbide.
Ceramic parts almost always have recessed inserts, with the edge protected by a chamfer, and require rigid, powerful, and fast machines.
CBN and PCD
These are the two hardest materials. They are sold as small plates brazed onto the corner of a carbide insert (or, for the more robust versions, as complete inserts).
- CBN, polycrystalline cubic boron nitride: It is the second-hardest material in existence after diamond and does not react with iron. It is a tool for hard turning (hardened steels ranging from 45 to 65 HRC, instead of grinding), hard cast irons, and sintered superalloys;
- PCD, polycrystalline diamond: extremely hard and with a perfect cutting edge, but at temperatures above 600–700 °C, it reacts with iron and wears down. It is used only on non-ferrous materials: aluminum (especially aluminum with a high silicon content), copper, brass, filled plastics, carbon fiber, wood, and graphite.
| Material | Hardness (HV) | Withstands temperatures up to approximately (°C) | Where it is used |
|---|---|---|---|
| High-Speed Steel (HSS) | 750-900 | 550-600 | drills, taps, milling tools, shaped tools |
| Hard metal | 1300-1800 | 900-1000 | almost everything: inserts, milling cutters, and solid-carbide drill bits |
| Cermet | 1500-1800 | 1000 | steel finishing |
| Al₂O₃ Ceramics | 1800-2200 | 1200 | cast iron and hardened steel, continuous cutting |
| Silicon nitride | 1500-1800 | 1200 | roughing of cast iron and superalloys |
| CBN | 3000-4500 | 1200 | hardened steels, hard cast iron |
| PCD | 6000-9000 | 650 | aluminum, copper, plastics, composites |
These are approximate and rounded values, prepared by CNC Simulator Italia to compare the product families. Within each family, there are significant differences between one grade and another.
25.6 CVD and PVD Coatings
Almost all inserts for steel, stainless steel, and cast iron are now coated: a very thin layer—just a few micrometers thick—of extremely hard ceramic compounds is deposited onto the carbide. The coating acts as a shield against wear and heat, while the carbide core beneath provides toughness. A good coating can extend the life of a cutting edge by 2 to 5 times, or allow for higher cutting speeds while maintaining the same service life. There are two processes.
- CVD (chemical vapor deposition): The layers form from gases that react on the surface at approximately 900–1050 °C. This process produces thick, multi-layer coatings—ranging from 5 to 25 µm in total thickness—with excellent wear and heat resistance. The downside is that the edge must be slightly rounded before coating; this method is the preferred choice for turning and milling steel and cast iron during roughing and semi-finishing operations;
- PVD (physical vapor deposition): The material is evaporated or “sputtered” from a cathode in a vacuum and deposited at approximately 400–550 °C. The layers are thin, ranging from 1 to 5 µm, and remain under compressive stress: the cutting edge stays sharp and tough. This is the material of choice for solid-body milling cutters and drills, positive inserts, stainless steel, superalloys, threading, parting off, and all tools that require a clean cut.
| Coating | Process | Typical thickness (µm) | Color | What is it used for? |
|---|---|---|---|---|
| TiN, titanium nitride | PVD and CVD | 1-4 | gold | universal, HSS, shows signs of wear |
| TiCN, titanium carbonitride | CVD and PVD | 2-10 | gray-blue, purple-gray | abrasion resistance, cast iron, steel |
| Al₂O₃, aluminum oxide | CVD | 2-10 | black or dark gray | heat barrier, high speeds on steel and cast iron |
| TiAlN, titanium aluminum nitride | PVD | 2-5 | dark purple, charcoal gray | high temperatures, dry cutting, stainless steel |
| AlTiN (more aluminum) | PVD | 1-4 | black, dark gray | hard and hardened steels, high-speed milling |
| DLC, diamond-like carbon | PVD | 0,5-3 | black, charcoal gray | aluminum, copper, plastics (not for steel) |
Approximate thicknesses and colors: Every manufacturer has its own formulas, and the color also depends on the lighting and thickness. Color alone is not enough to identify a coating; the quality code is the definitive indicator.
TiAlN and AlTiN have a special property: when heated, the aluminum on the surface oxidizes and forms a very thin oxide film that protects the layer beneath it. This is why they perform well in dry conditions and at high temperatures. DLC, on the other hand, is extremely smooth and glides easily over aluminum, but it degrades at temperatures above 350–400 °C: it’s not designed for use with steel.
25.7 Brazed and insert-type tools: ISO 1832 designation
Until a few decades ago, almost exclusively brazed tools were used on lathes: a carbide insert brazed with a silver or copper alloy onto the tip of a steel shank, which had to be resharpened on a grinding wheel when it wore down. They are still used for special-shaped tools, for specialized tasks, and in schools, but they have two drawbacks: with each sharpening, the geometry and position of the tip change, and the brazing leaves residual stresses that can cause the insert to crack.
Today, indexable insert tools (mechanically clamped inserts) are almost always used: the insert has multiple cutting edges that are already sharpened, coated, and feature a molded chipbreaker; when a cutting edge is worn down, the insert is turned (a process called “indexing”), and the new cutting edge is positioned exactly in the same spot, without having to remeasure the tool. When all the cutting edges are worn out, the insert is discarded (or rather: collected and recycled, since tungsten is very valuable).
Inserts are ordered using a code standardized by ISO 1832: seven mandatory digits, two optional digits, and—following a hyphen—the manufacturer’s code for the chipbreaker. Let’s take the world’s best-selling insert, the CNMG 120408-PM, as an example.
Position 1: Form
The first letter indicates the shape of the insert and the tip angle. The most commonly used shapes are: C (rhombus, 80°), D (rhombus, 55°), V (rhombus, 35°), T (triangle, 60°), W (trigonal, 80°—a triangle with cut corners), S (square, 90°), and R (round). There are also the shapes E (rhombus 75°), M (rhombus 86°), K (parallelogram 55°), A and B (parallelograms 85° and 82°), H (hexagon), O (octagon), P (pentagon), and L (rectangle).
Position 2: the rake angle
It is the angle between the side of the insert and the line perpendicular to the face. An insert with a 0° rake angle (N) is called negative: to prevent it from scraping against the workpiece, it must be mounted at an angle in the tool holder, but in return, it can be flipped and used on both sides, so it has twice as many cutting edges and is more durable. Inserts with a positive rake angle (B 5°, C 7°, P 11°) are called positive: they cut more easily, exert less force on the workpiece, and are used for finishing operations, thin workpieces, small boring bars, and low-power machines; however, they have only one cutting face.
| Letter | A | B | C | D | E | F | G | N | P |
|---|---|---|---|---|---|---|---|---|---|
| Strip | 3° | 5° | 7° | 15° | 20° | 25° | 30° | 0° | 11° |
Position 3: The tolerance class
It specifies the precision with which three measurements are made: the diameter d of the inscribed circle, the position m of the tip, and the thickness s. The M and U inserts are sintered and not ground along their periphery; they are the most economical and the most commonly used for roughing and medium-finish machining; the G, E, and C inserts are ground, with the tip precision within a few hundredths, for finishing, threading, and operations where the tip position matters.
| Class | d (mm) | m (mm) | s (mm) |
|---|---|---|---|
| C (revised) | ±0,025 | ±0,013 | ±0,025 |
| E (revised) | ±0,025 | ±0,025 | ±0,025 |
| G (revised) | ±0,025 | ±0,025 | ±0,13 |
| M (sintered) | from ±0.05 to ±0.15 | from ±0.08 to ±0.20 | ±0,13 |
| U (sintered) | from ±0.08 to ±0.25 | from ±0.13 to ±0.38 | ±0,13 |
Rounded values from the standard; for M and U, the tolerance increases with the size of the insert (for a 12.7 mm insert in class M: d ±0.08 and m ±0.13, approximately).
Position 4: the bit (hole and chip breaker)
The fourth letter indicates the design of the mounting hole and whether there are chip breakers on one side or both. The most common types are:
| Letter | Forum | Chip Breaker | Typical Use |
|---|---|---|---|
| N | no one | no one | Smooth inserts with brackets (ceramic, milling) |
| R | no one | on one side | top bracket |
| A | cylindrical | no one | flat lever inserts |
| M | cylindrical | on one side | single-sided negatives |
| G | cylindrical | on both sides | double-sided negatives (CNMG, DNMG, TNMG) |
| W | flared at a 40–60° angle on one side | no one | positive with a screw |
| T | flared at a 40–60° angle on one side | on one side | Positive-wound (CCMT, DCMT, VBMT) |
Positions 5, 6, and 7: the measurements
- Position 5, cutting edge length l in millimeters, without decimals (12 means 12.9 mm). For round inserts, this is the diameter;
- Position 6, thickness s: a two-character code, 02 = 2.38 mm, 03 = 3.18 mm, T3 = 3.97 mm, 04 = 4.76 mm, 06 = 6.35 mm (measurements are in fractions of an inch: 3/32", 1/8", 5/32", 3/16", 1/4");
- Position 7, nose radius rε in tenths of a millimeter: 02 = 0.2 mm, 04 = 0.4 mm, 08 = 0.8 mm, 12 = 1.2 mm, 16 = 1.6 mm. The milling inserts here have two letters, which indicate the setting angle and the rake face clearance.
The length of the cutting edge is derived from the inscribed circle based on the geometry of the rhombus or triangle (Chapter 3):
Positions 8 and 9 and the chip breaker
The two optional designations indicate the condition of the cutting edge (F sharp, E rounded, T with negative chamfer, S chamfered and rounded) and the hand (R right, L left, N neutral). After the hyphen, each manufacturer includes its own chipbreaker code: usually one letter from the ISO group and one for the type of operation, for example, F for finishing, M for medium, and R for roughing. The chipbreaker is the shape of the face that bends and breaks the chip: it is selected based on its working range (paragraph 25.14).
Three inserts all have the number 16 or 12 in the fifth position. What is their inscribed circle?
Position number 5 does not refer to the “size” of the insert but to the length of the cutting edge: when comparing inserts of different shapes, it is always best to look at the inscribed circle.
25.8 Select the shape and insert radius
Choosing an insert is always a trade-off between strength and accessibility. A drill bit with a large angle has a lot of material behind the cutting edge: it can handle high feeds and depths, interrupted cuts, and burrs. A narrow drill bit, on the other hand, can reach into profiles, grooves, and corners, but it breaks more easily and generates more heat.
- R, round: the most robust, excellent for heavy roughing, superalloys, and light finishing; with this type, the feed rate can be high because the chip becomes thinner;
- S, 90° square: extremely sturdy, for roughing and 45° chamfers, but does not allow for a 90° shoulder;
- C, 80° rhombic: the most commonly used; with the same tool, it rounds and faces against a shoulder (κr 95°), sturdy enough for roughing;
- W, 80° triangular: similar to C but with 6 negative cutting edges; excellent for light and medium roughing;
- T, 60° triangular: versatile and with many cutting edges, but the 60° tip is less sturdy than the C;
- D, 55° rhombic: for profiles with small undercuts and contours, for medium and finishing operations;
- V, rhombic 35°: the most versatile; fits into grooves and profiles with deep undercuts; for finishing only, using light passes.
The nose radius follows the same logic. A large radius (1.2 or 1.6 mm) makes the nose sturdy and allows for high feeds with good roughness, but it exerts more pressure on the workpiece and causes thin workpieces to vibrate. A small radius (0.2 or 0.4 mm) cuts lightly and is suitable for shallow passes and fragile workpieces. Two rules of thumb to use as a starting point:
- During roughing, the feed does not exceed approximately half the nose radius: with rε = 0.8 mm, a maximum of 0.4 mm per revolution;
- The cutting depth ranges from about 2/3 of the radius (below this point, the cutting edge skims the material instead of cutting it) to about 2/3 of the cutting edge length (above this point, there is a risk of breaking the insert).
C45 shaft to be turned and faced, ap = 4 mm, f = 0.35 mm/rev, heavy-duty lathe. We recommend a CNMG 120412 with a roughing chipbreaker, P25 grade with CVD coating. Is that okay?
Austenitic stainless steel pin with a semicircular groove, to be finished to ap = 0.5 mm and Ra 0.8 µm. The profile has an undercut; a narrow-fluted drill is required. A VBMT 160404 in M15 grade with PVD coating is selected.
Same feed rate f = 0.2 mm/revolution, three inserts with rε = 0.4, 0.8, and 1.2 mm. What is the resulting theoretical roughness?
To achieve a better surface finish without slowing down, you can use an insert scraping (wiper), which has a section near the tip with a much larger radius: at the same feed rate, this results in approximately half the roughness, or allows the feed rate to be doubled.
How much does a cutting edge cost?
An insert with more cutting edges costs more, but each cutting edge costs less. To compare different inserts, calculate the cost per cutting edge and the cost per workpiece:
A CNMG costs €12 and has 4 cutting edges; a DCMT costs €9 and has 2. Each cutting edge lasts for 15 minutes of cutting, and each workpiece requires 1.4 minutes of cutting.
For this reason, when the profile allows it, double-sided negative inserts are preferred. The cost of the insert, however, is usually a small fraction of the cost of the workpiece: an insert that lasts longer or allows for faster machining is worth the investment even if it costs twice as much (Chapter 30).
25.9 Tool holders: ISO 5608 designations and boring bars
Tool holders for external turning also have a standardized code, ISO 5608, which is formatted the same way as that for inserts. The most commonly used tool holder is the PCLNR 2525M12, which pairs with the CNMG 120408.
| Location | Meaning | Most Common Letters |
|---|---|---|
| 1 | locking system | C: Bracket from above (insert without hole) · M: Bracket and pin in the hole · P: Lever that pulls the insert out of the hole · S: Screw in the countersunk hole · D: Rigid bracket, double locking |
| 2 | shape of the insert | such as position 1 of the insert: C, D, S, T, V, W, R |
| 3 | type and registration angle κr | A 90° clockwise · F 90° to smash · J 93° · K 75th to show off · L 95° · N 63° · R 75° · S 45° · V 72,5° |
| 4 | insert template | such as position 2 of the insert: N, B, C, P |
| 5 | hand | R = Right · L = Left · N = Neutral |
| 6 e 7 | height h and width b of the stem | two digits each, in mm: 1616, 2020, 2525, 3225 |
| 8 | length l1 | H 100 · K 125 · M 150 · P 170 · Q 180 · R 200 · S 250 mm |
| 9 | insert size | cutting edge length, such as position 5 of the insert |
Boring bars
For internal turning, boring bars are used, designated according to ISO 6261 using the same logic. The code begins with the material and dimensions of the bar, followed by the section that holds the insert. For example, S20S-SDUCR11: steel bar (S), 20 mm in diameter, 250 mm long (S); screw clamping (S), D 55° insert, κr 93° (U), 7° rake angle (C), right-hand (R), 11 mm cutting edge. In catalogs, the first letter usually indicates the material: S for steel, A for steel with a coolant hole, C for cemented carbide, and E for cemented carbide with coolant.
A bar acts as a cantilever, like a simply supported beam (Chapter 10): under shear force, it deflects, and if the stick-out is too great, it vibrates and leaves the typical “flaked” surface on the wall. The rule of thumb is expressed as the ratio of the stick-out L to the diameter D of the bar:
| Barra | Approximate maximum L/D ratio | Notes |
|---|---|---|
| Steel | 3 (up to 4 with reduced parameters) | the cheapest |
| Solid carbide | 5 to 7 | about three times as rigid and expensive |
| Vibration dampener (damped) | 10 to 14 | contains an internal damping mass |
Approximate values for a rigid machine and a secure clamp on the bar (a sleeve or clamp that grips at least 3 or 4 diameters of the bar). Use the thickest possible bar and the shortest possible stick-out.
A Ø40 hole 110 mm deep must be drilled. The bar must protrude at least 110 + 5 = 115 mm. In a Ø40 hole, allowing room for chips, a Ø32 bar is the largest that will fit.
The Ø25 bar from the previous example protrudes 115 mm, and a radial force of 400 N acts on its tip. How much does it deflect if it is made of steel, and how much if it is made of cemented carbide?
The error doubles with respect to the diameter: the steel bar would leave the hole about 0.10 mm smaller at the bottom than at the entrance. That is why, during boring, light finishing passes are performed using a positive insert and a small radius, which exert little force.
25.10 Milling Tools
In milling, the workpiece remains stationary while the tool rotates; the tool has multiple cutting edges (teeth) that enter and exit the material with each revolution. The parameters and machining methods are covered in Chapter 27; here we will look at the different types of milling cutters.
End mills, toric mills, and ball-end mills
The end mill (in English end mill) cuts both on the side and at the tip: it performs shoulder cuts, grooving, pockets, and contouring. The most common types are solid tools made of micrograin carbide, PVD-coated, or HSS-Co for light-duty work. The number of teeth The choice depends on the material and the space required for the chips:
- 2 teeth: large flutes, chips clear easily; for aluminum, plastics, and solid bores; often with one tooth that cuts all the way to the center to allow for vertical cutting;
- 3 teeth: a universal compromise, widely used for machining aluminum at high speeds and for steel grooves;
- 4 teeth or more: thicker shank and therefore stiffer; for steel, stainless steel, and side finishing. With 6 or more teeth, hard steels are finished and trochoidal milling is performed.
The helix angle of the teeth, usually 30° or 45°, ensures a smooth, progressive cut; the cutters variable-pitch propeller have teeth spaced at different intervals to dampen vibrations. The toric drill bit has edges with a radius: the edge does not splinter, and the bottom of the pocket remains rounded by a fillet. The ball end mill It has a hemispherical head: it is the tool used for three-dimensional surfaces (molds, blades, free-form shapes) machined with closely spaced passes.
Indexable-insert cutters and special cutters
- Facing cutters (sleeve or insert type): steel bodies with diameters ranging from 40 to 250 mm and beyond, with 45° inserts (for fine chips and high feeds), 90° inserts (for shoulder milling), or round inserts (for heavy-duty roughing);
- disc cutters: discs with teeth on the periphery and sometimes on the sides (three-cut), mounted on a shaft; for grooves, slots, and cuts;
- T-slot cutters: a disc mounted on a thin shank that fits into the pre-milled slot and widens the bottom;
- chamfering cutters: 90° (or 60°, 120°) conical cutters, for chamfering edges and countersinking holes; they are often used as centering tools as well;
- threading cutters: cutters with a thread profile that, using helical interpolation (G02 or G03 with the Z-axis moving down one pitch per revolution), can cut both internal and external threads of any diameter with the same tool.
Regrinding Solid-Carbide End Mills
A solid carbide end mill costs anywhere from a few dozen to a few hundred euros and can be resharpened multiple times: the worn portion at the tip (and, if necessary, on the flank) is removed, the geometry is restored, and the coating is reapplied. With each resharpening, the cutter becomes shorter, and if the side is resharpened, the diameter decreases: it must be remeasured, and the depth gauge must be adjusted accordingly.
Carbide end mill, Ø12, with 26 mm-long cutting edges; for the deepest groove, at least 18 mm is required. Each time the cutting edge is resharpened, 0.4 mm is removed. A new cutter costs €85; a resharpening with a new coating costs €22; and 150 workpieces can be produced between resharpenings.
In practice, a re-sharpened cutter performs slightly worse than a new one, and it’s not always possible to reach 20 re-sharpenings; however, it’s still very cost-effective, especially for large and specialty cutters.
25.11 Drill bits, center punches, and reamers
The twist drill bit
The twist drill has two main cutting edges on the tapered tip, two helical flutes that carry the chips away, two chamfers (the edges) that guide it into the hole, and a transverse cutting edge at the center, where the two main cutting edges meet. The transverse cutting edge does not actually cut: it pushes and crushes the material, and is the cause of the high axial force and the drill bit’s tendency to wander at the start of the hole.
- Point angle σ: 118° is the standard angle for general-purpose HSS drill bits; 135° is used for hard steels and stainless steel and is almost always combined with a tapered shank, which shortens the transverse cutting edge and makes the drill bit have a chuck. Carbide drill bits usually have a point angle of 135° or 140°;
- Helix angle β: Type N from 25° to 35° for steel and cast iron; Type H from 10° to 15° for brass and hard plastics (does not “pull” into the material), type W from 35° to 45° for aluminum and soft materials;
- lip rake angle: 8° to 14° behind the main cutting edges; without a rake angle, the tip will not penetrate.
The length of the tapered drill bit is calculated as the height of a cone (Chapter 4, Section 4.6): this is used to determine how far the drill bit must penetrate to create a blind hole of a certain depth at full diameter.
Blind hole, Ø10, with a full diameter of 25 mm. How long is the tapered drill bit with a 118° HSS tip and a 135° carbide tip? At what Z-coordinate should the bottom of the hole be programmed?
The CNC controls the drill bit, not the full diameter: if you forget to account for h, the hole will be too short by exactly the length of the tapered drill bit.
Carbide Drills and Insert Drills
The solid carbide bits They drill 3 to 10 times faster than HSS, producing more precise and straighter holes. Almost all of them have internal holes for the coolant, which extends beyond the tip and pushes the chip out: on machining centers, they are used with coolant fed through the spindle at pressures ranging from 20 to 70 bar. For diameters of approximately 12 mm and larger, the following are also used: insert-tipped drills, with a central insert and a peripheral insert, for short holes (2 to 5 diameters): the bits are not resharpened; instead, the inserts are replaced; other bits have a replaceable head made of hard metal on a steel body.
Doilies and centerpieces
Two different tools with similar names:
- The center point (60° A-shape or tapered R-shape) forms the tapered seat for the lathe tailstock or for mounting the workpiece between centers; it has a small pilot point and a 60° taper;
- the doily (spot drill) at 90° or 120° creates a small indentation on the surface, so that the twist drill starts exactly at the right spot without veering off course. If the center punch has an angle slightly wider than that of the drill bit, the drill bit’s cutting edges will make contact first, rather than the cross-cutting edge; using a 90° center punch also creates a chamfer on the hole.
Reamers
The reamer brings a pre-drilled hole to its final size, with a tight tolerance (typically H7) and a good level of roughness. It has many straight or left-hand helical teeth, a short tapered shank, and removes a small amount of material: usually 0.1 to 0.3 mm from the diameter. Hand reamers have a long shank and a square shank end; machine reamers are used at low speeds and high feeds. Drilling, boring, and their parameters are covered in Chapter 28.
12/25 Taps, dies, and tools for threading on a lathe
Males
The tap threads the internal thread (the female thread) in a pre-drilled hole. It has a tapered entry, where the first threads are chamfered and cut gradually, and a calibrating section that sets the thread size. The flutes carry away the chips and coolant. The main types are:
- hand taps: these are used with a tap driver, often in sets of two or three (roughing tap, intermediate tap, and finishing tap, with progressively shorter shanks), or as a single workpiece for small diameters;
- Machine taps with right-hand threads (35° to 45°): the thread pulls the chips upward and out of the hole; these are used for blind holes, with a short lead (C-shape, 2–3 threads) to reach close to the bottom;
- taps with a pointed tip (correct entry, type B): straight flutes with an angled cut at the tip that pushes the chips forward, in front of the tap; these are for through holes, where the chips exit on the other side and do not clog the tap;
- Rolling taps (deformation taps): They have no grooves and do not cut, but displace the material using lobes; the thread is stronger, there are no chips, and the tap has a long service life, but they are only suitable for ductile materials (steels up to about 1200 N/mm², aluminum, copper), and the pilot hole must be larger than that required for cutting taps.
Supply Chains
The die is the opposite of the tap: a quick-release steel ring with internal threads and holes that act as grooves, used to thread screws and pins by hand. It is mounted in the die holder; those with a radial cut can be opened or tightened slightly with a screw to adjust the size. In production, screws are made by rolling (Chapter 23) or on lathes.
Tools for Threading on a Lathe
On a lathe, threads are formed using inserts with the thread profile (G76 or G92 cycle, Chapter 26). The most common inserts are “tilting” inserts, mounted in a tool holder that tilts them by the thread helix angle using shims. There are two types:
- Full-profile: The insert has the exact shape of a single-pitch thread, including the crest. The thread comes out with the correct base and crest, without burrs, and there is no need to turn the outer diameter with precision; however, one insert is required for each pitch;
- Partial-profile (60° or 55° V-tip): The insert cuts only the groove and has a small radius, making it suitable for the finest pitch in its range; a single insert can be used for multiple pitches, but the crest remains as turned, and the diameter must first be finished with precision.
The designation system for tapping inserts does not follow ISO 1832: each manufacturer has its own system, but almost all use a format such as “16ER 1.5 ISO,” meaning size 16, external (E), right-hand (R), pitch 1.5 mm, ISO metric profile. For the partial profile, the pitch is replaced by the angle and the pitch range.
25.13 Clamping and Fastening: Collets, Spindles, and Cones
A precision tool is of little use if it is mounted crookedly. Two factors determine the quality of a fastening: theeccentricity (runout), that is, how much the cutting edge wobbles as it rotates, measured with a dial indicator, and the clamping force, that is, how much torque can be transmitted without the tool slipping. Even a few hundredths of an inch of eccentricity causes one tooth to bear more of the load than the others and shortens the life of a milling cutter.
Spindles for Tools with Cylindrical Shanks
- ER spindles (ISO 15488): The collet is a sleeve with longitudinal slots and an 8° external taper; when the ring nut is tightened, the collet slides into the taper and clamps onto the shank. Each collet clamps a range of approximately 1 mm (for example, from 9 to 10 mm), and an ER32 collet chuck accommodates shanks from 2 to 20 mm. They are universal and economical; eccentricity ranges from 0.005 to 0.015 mm depending on the grade;
- Weldon spindles: The spindle has a flat surface against which a side screw presses. The cutter cannot slip or come loose, but the screw pushes it sideways, resulting in greater eccentricity; they are used for heavy-duty roughing and insert-tipped cutters;
- Thermal shrink-fit spindles: The spindle hole is a few hundredths smaller than the tool shank; the spindle is heated with an induction coil to approximately 300 °C, the tool is inserted, and as the spindle cools, it grips the tool all around. Eccentricity less than 0.003 mm, slender shape, high rigidity; a shrink-fit machine is required;
- Hydraulic spindles: A pressurized oil chamber deforms a thin sleeve that grips the shank; they are tightened with a single screw and a wrench, have an eccentricity of less than 0.003 mm, and dampen vibrations. Excellent for reamers and finishing operations.
The machine's spindle attachments
The tool holder attaches to the spindle of the milling machine or machining center via a taper. The dimensions and calculations for the tapers are provided in Chapter 6 (Section 6.2); here, we are interested in how they work.
- SK (DIN 69871, also known as ISO), BT (Japanese standard MAS 403) and CAT (Americans) all use the Steep slope 7:24 (a semi-angle of approximately 8.3°), drawn into the spindle by a tie rod screwed in all the way. The 7:24 cone doesn't lock into place on its own and comes off easily, but it touches only on the cone: There is a small gap between the flange and the spindle face. At high speeds, the spindle expands due to centrifugal force, and the cone moves in a little further: the Z-axis position changes, and the rigidity decreases. The most common sizes are 30, 40, and 50;
- HSK (DIN 69893, ISO 12164) uses a short, hollow 1:10 taper: internal collets pull it from the inside and expand it against the spindle, while the flange rests against the face. By making contact with both the cone and the face, the connection is rigid and precise in the Z-axis even at very high speeds, and tool changes are quick because the connection is short. Sizes are indicated by the flange diameter: HSK-A63, HSK-A100, and so on.
Balancing
A tool holder with the tool mounted is never perfectly symmetrical: the Weldon face, the screw, and the drive key shift the center of gravity off-axis. At high RPMs, this imbalance It generates centrifugal force that causes the spindle to vibrate, degrades the surface finish, and wears out the bearings. For spindles that rotate at high speeds (above about 8,000 rpm), thebalancing: The imbalance is measured using a special machine and corrected by removing material or adjusting the balancing screws. The required quality is indicated by the grade G According to ISO 21940-11 (formerly ISO 1940): G 2.5 or G 6.3 is typically required for tool holders.
An HSK-A63 tool holder with a milling cutter weighs 1.6 kg and rotates at 18,000 rpm. The required balance grade is G 2.5. How much unbalance can remain, and what is the resulting centrifugal force? What if the unbalance were 50 g·mm?
25.14 Presets, Offset Values, Tool Management, and Catalogs
Presets and Equalizers
The CNC must know where the tip of each tool is located: the length (and on the lathe, the X dimension as well), the radius of the milling cutter or the nose radius of the insert, and theorientation of the tip. These measurements are recorded in the table of correctors (offset). These can be entered on the machine by tapping a workpiece or a reference point, or off the machine using a preset bench: a device with a mount identical to that of the spindle and a camera or projector that measures length and diameter to the micrometer while the machine continues to operate. Measuring instruments (optical presetting, probes, and in-machine lasers) are covered in Chapter 37; how the control system uses length and radius compensators (G43, G41, G42) is covered in Chapter 50.
Maintaining and Resharpening Tools
- Part numbers and inventory: Each mounted tool (tool holder, collet, end mill) has a number, a data sheet with its dimensions, and a designated location in the machine’s tool magazine; many machining centers read the dimensions from a chip on the tool holder;
- Service life: The number of workpieces or minutes a cutting edge can last is determined, and it is replaced before it breaks; the control system manages tool life, with a second tool coming into use when the first one is worn out;
- Inserts: Turn all the cutting edges, check for wear (Chapter 24) to determine whether the parameters are acceptable, and collect the used ones for recycling;
- Regrinding: end mills, drill bits, reamers, and solid taps are sent to a grinder, which restores their original geometry and coating; HSS tools can also be resharpened in the workshop using a grinding wheel, ensuring the correct angles are maintained; after each resharpening, the tool is remeasured;
- Cleaning: Cones and collets must be kept clean and free of burrs; a single chip in the spindle cone is enough to cause an eccentricity of a few hundredths.
How to Read a Catalog
Manufacturers’ catalogs are extensive, but they’re all structured the same way. You start with the workpiece material (ISO group and subgroup) and the type of machining operation (roughing, semi-finishing, finishing, stable or difficult conditions); the catalog then suggests the grade and the chipbreaker. On the insert pages, next to each part number, you’ll find a drawing with dimensions, the available grades (marked with a dot or symbol for those in stock), and the chipbreaker’s operating range: the depth and feeds at which the chip breaks effectively. Finally, a table provides the starting cutting speed for each grade and material, often based on the feeds. The tool holder is selected from its corresponding page, ensuring it is compatible with the chosen insert.
Using the CNMG 120408 insert, two operations must be performed on a Ø50 shaft made of C45 steel: a pass A with ap = 3 mm and f = 0.25 mm/revolution, and a pass B with ap = 0.5 mm and f = 0.1 mm/rev. The M chipbreaker has an f range of 0.12–0.45 mm/rev and ap 0.8–5 mm; for the selected grade, the catalog recommends Vc = 230 m/min.
25.15 The Formulas in This Chapter
| What Are You Looking For? | Formula | Units |
|---|---|---|
| Cutting edge of a rhombic insert | l = d / sin ε | mm |
| Cutting edge of a triangular insert | l = d · √3 | mm |
| Theoretical Roughness (from 26.10) | Ra ≈ 1000 · f² / (31,2 · rε) · Rt = 1000 · f² / (8 · rε) | µm |
| Feed rate for one pass of roughness | f = √(31,2 · rε · Ra / 1000) | mm/revolution |
| Cost per cutting edge and per workpiece | Ct = Ci / zt · Cp = Ct / Np | € |
| Deflection of a Cantilever Beam | f = F · L³ / (3 · E · I) · I = π · D4 / 64 | mm |
| Number of resharpenings | Nr = (Lu − Lmin) / ΔL | number |
| Cost per workpiece, including regrinding | Cp = (Cn + Nr · Cr) / ((Nr + 1) · Z) | € |
| Length of the tapered tip | h = D / (2 · tan(σ/2)) ≈ 0.30 · D for 118° | mm |
| Permitted Imbalance | e = 9549 · G / n · U = e · m | g·mm/kg · g·mm |
| Centrifugal force due to imbalance | F = U · 10−6 · ω² · ω = 2 · π · n / 60 | N |
25.16 Exercises
Try to solve them on your own, using a calculator and the tables in this chapter, before looking at the solutions.
Solution
T triangular 60°, N clearance 0° (negative), M tolerance M, G hole and chipbreaker on both faces. 16: l = 9.525 · √3 = 16.50 mm, inscribed circle 9.525 mm; 04 thickness 4.76 mm; 08 radius 0.8 mm. Cutting edges: 3 points per face × 2 faces = 6.
Solution
V rhombic 35°, B clearance 5° (positive), M tolerance M, T countersinked hole and chipbreaker on one face (screw-mounted). 16: l = 9.525 / sin 35° = 16.61 mm; 04 thickness 4.76 mm; 04 radius 0.4 mm. Two cutting edges. This is a finishing insert for profiles with undercuts and grooves, for light passes.
Solution
l = 9.525 / sin 80° = 9.525 / 0.9848 = 9.67 mm → “09”; thickness 3.18 → “03”; radius 0.8 → “08”. Code: CNMG 090308.
Solution
S: screw-lock, V: 35° rhombic inserts, J: κr = 93°, B: inserts with 5° rake angle, R: right-hand, shank 25 × 25 mm, M: length 150 mm, 16 cutting edges, each 16 mm. Fits VBMT 1604.. inserts, for example the VBMT 160404 from Exercise 2.
Solution
f² · 1000 = 0.0144 · 1000 = 14.4. Rt = 14.4 / (8 · 0.4) = 14.4 / 3.2 = 4.5 µm; Ra = 14.4 / (31.2 × 0.4) = 14.4 / 12.48 = 1.15 µm. Yes, that’s well below 1.6 µm.
Solution
Steel: 3 × 16 = 48 mm, which is too short. Carbide: from 5 × 16 = 80 mm to 7 × 16 = 112 mm, so 75 mm is fine. The required ratio is L/D = 75 / 16 = 4.7: the carbide bar is needed.
Solution
118°: h = 12 / (2 · tan 59°) = 12 / 3.3287 = 3.61 mm. 135°: h = 12 / (2 · tan 67.5°) = 12 / 4.8284 = 2.49 mm. Depth with the 135° bit: Z = −(30 + 2.49) = −32.49 mm, i.e., Z−32.5.
Solution
Ct = 10.80 / 6 = 1.80 € per cutting edge; Cp = 1.80 / 8 = 0.225 €, approximately 0.23 € per workpiece.
Solution
No. = (40 − 28) / 0.6 = 20 resharpenings. Without resharpening: 60 / 300 = 0.20 € per hole. With regrinding: (60 + 20 × 12) / (21 × 300) = 300 / 6,300 = 0.048 € per hole, about a quarter.
Solution
a) K, higher numbers (K20–K30), tough; b) M, lower numbers (M10–M15), PVD coating; c) S, S-class cemented carbide or ceramic; d) H, with a CBN insert.
Solution
e = 9,549 × 2.5 / 24,000 = 23,872.5 / 24,000 = 0.995 g·mm/kg; U = 0.995 × 0.8 = 0.80 g·mm.
Solution
The reduction is calculated using L³: (90 / 60)³ = 1.5³ = 3.375, more than three times. It is calculated using 1/D4: (25 / 20)4 = 1,254 = 2.44, so it decreases by a factor of 2.44.