Grinding and Finishing
When the workpiece is hardened, when the tolerance is reduced to just a few micrometers, or when the surface must be nearly mirror-like, a cutting tool alone is no longer sufficient: we turn to the grinding wheel. In this chapter, we’ll look at how a grinding wheel is made and how to interpret its designation, the speed at which it should rotate, and how to mount it safely; we’ll also cover the main types of grinding machines and their cycle times, dressing, common defects, and the allowance to leave; and finally, the machining operations that go even further: lapping, sanding, superfinishing, and polishing.
29.1 Why Corrections Are Made
Grinding is a material removal machining operation performed using a grinding wheel—that is, a disc composed of countless extremely hard grains held together by a binder. It is almost always used as the final operation, following turning or milling, and often after heat treatment. There are three reasons for grinding:
- The material is hard: hardened steel at 60 HRC (Chapter 19) or cemented carbide cannot be machined well with standard tools, while abrasive grains are much harder than any steel. Furthermore, heat treatment causes deformation of the workpiece (Chapter 22), and grinding removes precisely that deformation;
- The tolerance is tight: grinding typically achieves IT5 and IT6 grades (Chapter 14), meaning a few micrometers over a diameter of a few tens of millimeters, and shape errors (roundness, cylindricity, flatness) are also corrected;
- The surface roughness is low: standard grinding yields an Ra value ranging from 0.2 to 1.6 µm, with peaks of 0.05 µm in the most carefully finished surfaces (Chapter 16).
Then there are machining operations that are best performed with a grinding wheel rather than any other tool: sharpening tools, precision profiling of threads and teeth, bearing races, and the large flat surfaces of molds and plates. The trade-off is time: the grinding wheel removes only a few hundredths of a millimeter per pass, so first, almost all the material is removed with tools with cutting edges, and only a small allowance of material is left for the grinding wheel (section 29.13).
29.2 How a Grinding Wheel Works
A lathe tool has a single cutting edge with a precise shape and angles. A grinding wheel has millions of them—tiny and randomly arranged—which are the edges of the abrasive grains protruding from the surface. Each grain that passes over the workpiece removes a minuscule chip, often just a few micrometers thick and a few tenths of a millimeter long. Between the grains are the binder, which holds them together like tiny bridges, and the pores—empty spaces that collect the chips and carry coolant to the contact area.
This method of work gives rise to the characteristics of the grinding process:
- Very negative rake angles: the grains have random shapes and usually “push” the material rather than cut it. Many grains simply scrape the surface without removing any material. For this reason, the energy required to remove one cubic millimeter of steel is 5 to 20 times that of turning;
- A lot of heat: almost all of that energy is converted into heat, and a large portion (often more than half) is absorbed by the workpiece instead of being carried away with the chips, as happens on a lathe. In the contact zone, the temperature easily exceeds 1000 °C for an instant: you can see sparks, which are incandescent chips. Heat is the number one enemy of grinding (section 29.12);
- extremely high speed: the grinding wheel rotates at 30–35 m/s, or 1,800–2,100 m/min, which is ten times the cutting speed of a carbide insert;
- Self-sharpening: When a grain wears down and becomes rounded, the force acting on it increases until it either breaks, exposing new edges, or detaches from the binder, revealing the grains beneath. A well-chosen grinding wheel renews itself as it works.
29.3 Abrasives
The abrasive must be harder than the material being machined, withstand heat without softening, and not react chemically with the workpiece. Almost all grinding wheel abrasives are synthetic and are divided into conventional abrasives (corundum and silicon carbide) and superabrasives (CBN and diamond).
- Corundum (aluminum oxide, Al2O3, acronym A): the most commonly used abrasive for steels. Regular corundum (brown, about 95% oxide) is tough and works well for unhardened steels and roughing; the white corundum (over 99%, often abbreviated as WA) is more brittle, self-sharpens better, and generates less heat: it is the choice for hardened steels, tool steels, and high-speed steel. There are also pink corundum (with chromium) and ceramic corundums or sintered, with microcrystalline grains that break into very small pieces and last much longer.
- Silicon carbide (SiC, abbreviated as C): harder and more brittle than corundum. The black variety is used for cast iron, nonferrous metals (aluminum, brass, copper), rubber, plastic, and stone; the green variety, which is purer, was the traditional grinding wheel for sharpening hard metal and is used for ceramics. It does not work well on steels because it reacts with iron when hot.
- Cubic boron nitride (CBN, code B): the second-hardest material after diamond and, unlike diamond, it does not react with iron. It is the superabrasive of choice for hardened steels, high-speed steels, and nickel superalloys. A CBN grinding wheel is expensive, but it lasts tens or hundreds of times longer than a corundum wheel and experiences very little change in diameter: ideal for mass production.
- Diamond (abbreviation D): the hardest of all. It is used for hard metal, ceramics, glass, stone, composites, and for dressing other grinding wheels (paragraph 29.11). It is not used on steels: at temperatures above approximately 700 °C, the carbon in the diamond dissolves into the iron, and the grit wears down quickly.
| Abrasive | Acronym | Knoop hardness (approx.) | It is used for |
|---|---|---|---|
| Standard corundum | A | 2000 | unhardened steels, roughing, grinding |
| White corundum, ceramic | A (WA, SG...) | 2100 | hardened steels, tool steels, high-speed steel |
| Silicon carbide | C (green GC) | 2500 | cast iron, non-ferrous metals, plastic, stone, ceramics |
| CBN | B | 4500 | hardened and high-speed steels, superalloys, mass production |
| Diamond | D | 7000 | hard metal, ceramics, glass, composites, burnishers |
Approximate and rounded values. The Knoop hardness test is a microhardness test similar to the Vickers test (Chapter 19); for comparison, a steel hardened to 60 HRC has a Knoop hardness of around 700–750 HK.
29.4 The Grinding Wheel: Grit Size, Binder, Hardness, and Structure
Two grinding wheels made of the same abrasive can behave completely differently. In addition to the abrasive, a grinding wheel is defined by four characteristics: the size of the grains (grit), what holds them together (bond), how firmly they are held (hardness), and how densely packed they are (structure).
The Grain
Grit size is a number that indicates the size of the grains: it is the number of mesh openings per inch in the sieve used to sort them. Therefore, the higher the number, the finer the grains. As a very rough estimate, the average grain diameter in millimeters is approximately 15 divided by the mesh number.
| Grana | Medium grain size (mm, approx.) | Class | Typical Use |
|---|---|---|---|
| 24 | 0,76 | big | deburring, grinding, cutting |
| 36 | 0,53 | big | heavy roughing, grinding of castings |
| 46 | 0,37 | average | Roughing, large surfaces |
| 60 | 0,26 | average | The most commonly used grit: general round and flat grinding |
| 80 | 0,19 | end | finishing, tool sharpening |
| 100 | 0,13 | end | fine finishing, profiles |
| 120 | 0,11 | end | thin profiles, threads |
| 150 | 0,08 | very fine | very fine finishing, closely spaced threads |
| 180 | 0,07 | very fine | special finishing |
| 220 | 0,06 | very fine | special finishing, sanding |
Approximate average values, rounded. Grit sizes of 230 and above (microgrits, up to 1200 and beyond) are used for grinding, superfinishing, and lapping. For superabrasives, the grain size is specified directly in micrometers: B126 is CBN with a grain size of approximately 126 µm (section 29.5).
The rule is simple: coarse grit for removing a lot of material quickly and for soft, “sticky” materials; fine grit for smooth finishing, sharp edges, and thin profiles, as well as hard and brittle materials. With a finer grit, the roughness improves, but the grinding wheel clogs up sooner and gets hotter.
The binder
| Acronym | Binder | Features | Typical speed (m/s) | Usage |
|---|---|---|---|---|
| V | vitrified (ceramic) | rigid, porous, resistant to water and oil, polishes well; fragile when subjected to impact | 30–35, special editions up to 60 | most precision adjustments |
| B | resinoid (synthetic resin) | elastic and impact-resistant; is sensitive to alkaline coolants and ages | 45-80 | grinding, cutting, roughing, superabrasives |
| R | rubber | very elastic, glossy, and “complements” the workpiece | 35-50 | centerless grinding wheels, thin-section cutting, polishing |
| M | metallic (bronze, nickel) | extremely durable, long-lasting, difficult to revive | up to 100 and beyond | Diamond and CBN: glass, stone, hard metal, profiles |
Approximate values. The maximum speed stamped on the grinding wheel always takes precedence (paragraph 29.6). There are also fabric-reinforced resin-bonded (BF) abrasives for cutting discs and angle grinders.
Hardness
The hardness of a grinding wheel is not the hardness of the abrasive; it is the force with which the binder holds the grains in place. A hard grinding wheel retains the grains for a long time, even when they are worn down; a soft grinding wheel releases them quickly, always exposing new, cutting edges. It is indicated by a letter: from A (very soft) to Z (very hard).
| Letters | Hardness | When to use |
|---|---|---|
| A B C D | extremely tender | special cases |
| E F G | very sweet | Face grinding of hard materials, large contact surfaces |
| H I J K | tender | hardened steels, internal grinding, tangential surface grinding, sharpening |
| L M N O | average | Centerless cylindrical grinding of unhardened steels |
| P Q R S | hard | soft materials, deburring, small grinding wheels with close contact |
| T U ... Z | very hard | Heavy deburring of castings, hand grinding |
The practical rules are, somewhat surprisingly, reversed: hard material, soft grinding wheel (the grains wear down quickly and must fall off to make room for new ones); soft material, hard grinding wheel. Furthermore, the larger the contact surface between the grinding wheel and the workpiece (face grinding, internal grinding), the softer the grinding wheel must be, because many grains are working together and heat builds up. A grinding wheel that is too hard “vitrifies”: the worn-out grains remain stuck to it, and the smooth wheel scrapes, heats up, and burns the workpiece. A grinding wheel that is too soft wears down quickly and loses its shape.
The Facility
The structure is a number that indicates how close the grains are to one another: low numbers (0 to 3) indicate a closed grinding wheel, with densely packed grains and small pores; high numbers (8 to 14 and above) indicate an open grinding wheel, with large pores. A grinding wheel consists of three components: grains, binder, and pores, and their combined volumes total 100%. Many manufacturers use a rule of thumb: at structure 0, the grains occupy about 62% of the volume, and each additional number reduces this by about 2%.
Let's compare a grinding wheel with a structure of 5 (medium) to one with a structure of 8 (open), both made of the same abrasive and having the same hardness.
An open-face grinding wheel removes chips more effectively, and the coolant reaches where it’s needed: it’s the best choice for large contact surfaces, materials that tend to stick, and when the workpiece is prone to burning. A closed-face grinding wheel holds its shape better: it’s the best choice for profiles, edges, and fine finishing.
29.5 The Designation and Shapes of Grinding Wheels
Each grinding wheel has a label (often printed on the cardboard insert placed between the wheel and the flange) with its designation. The order of the information is specified by ISO 525: shape, dimensions, abrasive, grit size, hardness, structure, bonding agent, and maximum speed. Some entries include a manufacturer’s prefix or suffix (a number before the abrasive, a code after the bond), which indicates the exact type of grit or bond from the manufacturer’s catalog.
The label on a new grinding wheel reads: 1 · 300 × 40 × 76.2 · 89A 60 K 5 V 217 · 35 m/s. What kind of grinding wheel is this, and what is it used for?
For CBN and diamond grinding wheels, the designation is different: the abrasive is a thin layer (the crown) bonded or sintered onto a body made of aluminum, steel, or resin. The abrasive is specified by its grit size in micrometers (B126, D91), its concentration (C100 means 4.4 carats of abrasive per cubic centimeter of the crown, C75 means three-quarters of that, and so on; one carat equals 0.2 g), the binder, and the thickness of the crown.
Shapes
The standard assigns a number to each shape. The most common ones in the workshop are these:
- Type 1, flat: the straight grinding wheel used in cylindrical grinding, tangential flat grinding, centerless grinding, and bench grinders. The edge can be profiled as V-shaped, with a radius, or stepped;
- Type 5 and Type 7, lowered on one or both sides: like the flat type, but with space for flanges or to get close to a shoulder on the workpiece;
- Type 6 and Type 11, cup-style cylindrical and conical: they work with the face grinding wheel; they are used in face grinding and in tool sharpening;
- Type 12, flat: thin crown, designed to reach into the grooves between the teeth of milling cutters and tools to be sharpened;
- Type 27, concave, and Type 41, cutting disc: discs for portable angle grinders, for deburring and cutting.
Dimensions are always written in the order D × T × H (outer diameter, thickness, hole), with the addition, for cups, of the wall thickness W and the bottom thickness E. Typical diameters: 200 to 500 mm for cylindrical and surface grinding, 500 to 600 mm for centerless grinding, and a few millimeters to 100 mm for internal grinding.
29.6 Grinding Wheel Speed, Workpiece Speed, and Safety
The speed of the grinding wheel is its peripheral speed vs, the speed of a point on its edge. It’s the same concept as the cutting speed on a lathe (Chapter 26), but for the grinding wheel it’s expressed in meters per second. The formula for revolutions per minute from Chapter 26 therefore becomes, with 60 passed from minutes to seconds:
Typical speeds are 30–35 m/s for standard vitrified grinding wheels. With specially designed grinding wheels and machines (high-speed grinding), speeds reach 45–60 m/s and beyond, and with metal-bonded or electroplated CBN grinding wheels, speeds can even reach 100–150 m/s. Grinding wheels rated for speeds over 50 m/s are identified by one or more colored stripes on their surface (for example, blue for 50 m/s, yellow for 63, red for 80, and green for 100). Portable grinders use resin-bonded discs rated at 80 m/s.
A new grinding wheel with a diameter of 300 mm must operate at 35 m/s. How many revolutions per minute should the grinding wheel spindle rotate at?
After numerous dressings, the grinding wheel in Example 29.3 has shrunk to Ø250, but the spindle still rotates at 2,228 rpm. At what speed is it operating? How many revolutions would it take to return to 35 m/s? And what happens if you forget about the high RPM and install a new Ø300 grinding wheel?
For this reason, many modern grinding machines automatically adjust the speed based on the measured diameter of the grinding wheel (constant peripheral speed), and when the grinding wheel is changed, the program restarts at the speed of the new grinding wheel.
A bench grinder has a motor that runs at a fixed speed of 2,100 rpm. There is a Ø350 grinding wheel in stock stamped with “35 m/s.” Can it be installed?
Workpiece speed and speed ratio
The workpiece also moves: during cylindrical grinding, it rotates; during surface grinding, it moves along with the table. Its speed, vw, is much lower than that of the grinding wheel and is given in m/min, as on a lathe: 10 to 30 m/min for cylindrical and surface grinding, and 20 to 40 m/min for internal grinding. The workpiece’s rotational speed is calculated using the formula from Chapter 26: nw = 1000 · vw / (π · d).
What matters more than the two speeds alone is their ratio, q. If q is high (slow workpiece), each grain removes a thinner chip: the grinding wheel wears less and behaves like a harder wheel, the surface becomes smoother, but heat builds up. If q is low (high-speed workpiece), the chips are thicker; the grinding wheel wears down more quickly and behaves like a softer wheel, and the workpiece generates less heat.
| Correction | Steel | Cast iron |
|---|---|---|
| External Cylinder | 100-125 | 80-100 |
| Internal | 60-80 | 50-65 |
| Ring Road Plain (including the suburbs) | 60-80 | 50-65 |
| Front face (with cup wheel) | 40-60 | 30-50 |
Approximate values for the q ratio prepared by CNC Simulator Italia. Where the contact surface is larger (internal, front), the value is lower to prevent overheating.
A shaft with a diameter of 50 mm is being cylindrical ground at a feed rate of 20 m/min. How many revolutions per minute does the workpiece-holding head rotate at?
In Example 29.6, the grinding wheel operates at 35 m/s. What is the resulting q ratio? If, instead, you want q = 125 with the grinding wheel at 33 m/s on a Ø40 shaft, what speed and rotational speed should be applied to the workpiece?
Grinding Wheel Safety
A Ø300 vitrified grinding wheel rotating at 35 m/s has enormous energy and behaves like glass: if it breaks, the workpieces fly off at more than 120 km/h. The safety rules (Chapter 51 for machinery in general) are few but strict:
- Never exceed the maximum speed stamped on the grinding wheel, or the maximum RPM if specified; check the spindle speed before mounting a new grinding wheel (examples 29.4 and 29.5);
- Sound test on vitrified grinding wheels before installation: Hang the grinding wheel by the hole and tap it lightly with a wooden or plastic mallet. A sound grinding wheel produces a clear, metallic sound; a cracked grinding wheel produces a dull sound and should not be installed. Grinding wheels that have been dropped or struck must be discarded;
- Mount using matching flanges, with a diameter of at least one-third that of the grinding wheel, centered so that they clamp only on one rim; place cardboard spacers—compressible paper discs that distribute the pressure—between the grinding wheel and the flanges (these are usually the labels themselves). The grinding wheel must fit onto the spindle without forcing it; the nut is tightened just enough, without using extensions;
- Always keep the guard in place, with the opening as small as possible; on bench grinders, the workpiece rest should be adjusted very close to the grinding wheel (just a few millimeters) to prevent the workpiece from getting stuck;
- Balancing: An unbalanced grinding wheel vibrates, leaves marks on the workpiece, and causes wear on the spindle. It is balanced statically by moving the counterweights on the flange while the grinding wheel is mounted on a balancing stand, or on the machine using automatic balancers; this process is repeated after installation and after the first dressing;
- Initial startup: Run the machine idle for at least one minute at operating speed, with the guard in place and no one in the area of the grinding wheel; always wear safety glasses or a face shield; never work with the side of a flat grinding wheel. Resin-bonded grinding wheels have an expiration date because the binder ages.
29.7 Tangential Planar Grinding
In the tangential surface grinding The flat grinding wheel works with the periphery and the workpiece, which is usually clamped onto the magnetic board, moves back and forth beneath her. With each reversal, the table (or the grinding wheel head) shifts to one side of thelateral feed fa; when the grinding wheel has covered the entire width of the workpiece, it lowers by pass depth ap And here we go again. The surfaces become flat and parallel, with straight grooves running in the direction of travel.
To calculate the time, count the travels. The longitudinal travel Lc is the length of the workpiece plus an exit section on each side (usually 10–25 mm), so that the grinding wheel exits the workpiece completely. If the grinding wheel starts and ends with half its width extending beyond the edges, the transverse travel is approximately equal to the width B of the workpiece, and the number of longitudinal travels required to cover it is B / fa.
At the end of the finishing process, two or three empty passes are always made—that is, without lowering the grinding wheel: the machine, the workpiece, and the grinding wheel have flexed slightly under the stress, and these passes remove the final bit of material until almost no sparks are produced (known as spark-out in English). This improves flatness and roughness.
A 300 × 120 mm hardened plate has 0.2 mm of allowance on the top surface. Flat grinding wheel, Ø250 × 25. Rough-machine 0.17 mm with ap = 0.02 mm and fa = 12 mm (approximately half the grinding wheel); finish the remaining 0.03 mm with ap = 0.005 mm, fa = 6 mm, and 2 dry passes. Table speed: 18 m/min, 20 mm travel per side.
When the surfaces are large, instead of a flat grinding wheel, a cup wheel or segmented wheel who works across the street (front surface grinding): It removes much more material, but the contact surface is large, it generates more heat, and requires a softer, more open grinding wheel. The grooves form intersecting arcs.
29.8 External Cylindrical Grinding Between Centers
In external cylindrical grinding (or round grinding), the workpiece is supported between the centers of the workhead and the tailstock, and is rotated by a flange (the “flange drive”) driven by the workhead. The centers do not rotate with the workpiece (fixed centers); thus, any errors in the head bearings are not transferred to the workpiece, and the roundness depends solely on the workpiece centers. For this reason, the centers are made with care and, in the case of hardened workpieces, are re-machined after heat treatment. Short workpieces can also be held in a chuck or a collet.
There are two ways to do this:
- Longitudinal feed: the table moves the workpiece back and forth in front of the grinding wheel; at each end of the travel, the grinding wheel advances toward the workpiece by a depth of ap. This method is used for surfaces longer than the width of the grinding wheel;
- Plunge grinding (or full-width grinding): The grinding wheel, which has the same width as or is wider than the surface to be ground, advances in a radial direction without moving along the axis. This method is faster and leaves only circular grooves (useful for seal ring seats, Chapter 16), but the grinding wheel must be wider than the surface, and the shape of the grinding wheel is transferred to the workpiece.
Longitudinal Pass: Feeds and Time
The longitudinal feed f is given in millimeters per revolution of the workpiece, as a fraction of the grinding wheel width T: from 2/3 to 3/4 of T during roughing, and from 1/4 to 1/2 of T during finishing, so that every point on the workpiece passes under the grinding wheel multiple times. When both ends are free, the grinding wheel extends beyond each end by about one-third of its width: the center of the grinding wheel thus travels a distance of L − T/3. The depth of each pass is specified in terms of the radius, while the allowance is almost always measured in terms of the diameter: be careful not to confuse the two.
A pin has 0.5 mm of allowance on its diameter. 0.04 mm is left on the diameter for finishing; roughing is done with ap = 0.02 mm, the finishing process with ap = 0.005 mm. How many passes are needed?
A hardened shaft with a diameter of 40 is ground over a length of 200 mm (open ends), with a diameter reduction of 0.4 mm. Grinding wheel Ø400 × 40 at 35 m/s; vw = 20 m/min. Roughing: 0.35 mm off the diameter with ap = 0.02 mm and f = 25 mm/rev. Finishing: 0.05 mm off the diameter with ap = 0.005 mm, f = 10 mm/rev, and 2 idle travels.
The table moves at 4 m/min during roughing: each point on the workpiece passes under the grinding wheel 40 / 25 = 1.6 times per travel. During finishing, with f = 10 mm/rev, it passes under the wheel 4 times.
Plunge Grinding: Radial Feed and Time
During plunge cutting, the grinding wheel advances toward the workpiece axis at a speed vfr in mm/min, which is calculated from the radial feed per revolution of the workpiece fr: from 0.002 to 0.005 mm/revolution during roughing, and from 0.0005 to 0.001 during finishing. A typical cycle includes a short approach phase at roughing speed (the grinding wheel starts a few hundredths of a second before the workpiece, because the blank is never perfect), roughing, finishing, and a few seconds to allow the sparks to die down. To compare different cycles, the specific material removal rate Q'w is used—the volume removed per second per millimeter of grinding wheel width.
A Ø35 diameter 20 mm wide has 0.3 mm of allowance on the diameter. vw = 25 m/min. The cycle: 0.05 mm of approach and 0.12 mm of roughing (on the radius) at fr = 0.003 mm/rev, 0.03 mm of finishing at fr = 0.001 mm/rev, 3 s of cool-down.
Check: 0.12 + 0.03 = 0.15 mm on the radius, which is exactly 0.3 mm on the diameter. With CBN grinding wheels and rigid machines, a Q'w of 10 or higher can be achieved.
29.9 Internal Grinding and Centerless Grinding
Internal Grinding
In the internal grinding The holes are finished: the workpiece rotates, held in a self-centering chuck or a collet, and a small grinding wheel, mounted on a long shank, spins very fast inside the hole and moves back and forth along the axis. The grinding wheel has a diameter of about 0.7–0.8 times the diameter of the hole: If it were smaller, it would spin too fast; if it were larger, the contact arc would become too long and the workpiece would overheat. To achieve 25–30 m/s with such small grinding wheels, you need electric spindles capable of tens of thousands of revolutions per minute; the long, thin shank flexes, so you work with light passes, a soft grinding wheel, and often more dry passes.
A Ø30 hole is being ground in a hardened ring. Which grinding wheel should be chosen, and how many revolutions are needed to achieve 30 m/s? The electric spindle reaches 24,000 rpm: what is its actual operating speed? With the workpiece moving at 30 m/min, what are the values of nw and q?
Centerless Grinding
In centerless grinding, the workpiece is not held between centers or in a chuck: it rests on a blade (the support, with an inclined upper surface) between two grinding wheels. The large cutting wheel rotates rapidly (30–35 m/s) and removes material; the rubber drive wheel (or regulating wheel) rotates slowly in the same direction and, through friction, causes the workpiece to rotate at the same peripheral speed, thereby slowing it down. The center of the workpiece is positioned slightly higher than the line connecting the centers of the two grinding wheels (by about half the workpiece’s diameter, at most about fifteen millimeters): if it were at the same height, the workpiece might come out “round with three lobes,” with a constant diameter but not perfectly round.
If the drive wheel is tilted by a small angle α (from about 1° to 5°) relative to the workpiece axis, its peripheral speed has a component along that axis that pushes the workpiece forward: this is through-feed grinding, in which pins, rollers, shafts, and bars enter on one side and exit finished on the other, without stopping the machine. With α approximately zero and the workpiece held against a stop, plunge grinding is used instead, even on workpieces with shoulders or profiles.
Ø20 pins, 60 mm long, are ground through a through-feed machine. The drive wheel has a diameter of Ø250, rotates at 40 rpm, and is inclined at 3°. At what feed rate do the workpieces move? How many are produced per minute if they enter one after another?
Using the data from Example 29.13, how many revolutions does the spindle make, and at what peripheral speed? What is the ratio q for the grinding wheel operating at 35 m/s?
To move the workpieces faster, you increase α or nr; however, increasing nr also increases vw, and q decreases. For this reason, feeds are primarily adjusted by changing the angle.
29.10 Profile Grinding and Tool Sharpening
A grinding wheel can be profiled (Section 29.11) to have the exact shape desired for the workpiece: a radius, a V-shape, a thread profile, or an involute profile. This is how profile machining operations are performed:
- plunge-cut profile grinding, whether round or flat: grooves, radii, shoulders, and cones are machined in a single pass, with the grinding wheel cutting the workpiece’s profile in relief. This is the fastest way to grind workpieces with multiple diameters in a production run;
- Thread grinding: ball-screw drives, threaded gauges, taps. The grinding wheel, profiled with a single thread or multiple threads, is inclined at the helix angle, and the workpiece advances by one pitch per revolution, as in threading on a lathe (Chapter 26);
- gear grinding: case-hardened and quenched gears (Chapter 22) using profile grinding wheels or worm grinding wheels;
- Coordinate and profile grinding using optical guidance: for molds and dies, using very small grinding wheels that follow a programmed profile, similar to a milling cutter.
CNC grinding machines move the grinding wheel in the X and Z directions like a lathe and can follow any profile using a simply shaped grinding wheel: the program, apart from the speeds, is very similar to that of a CNC lathe (Chapter 50).
Tool Sharpening
Sharpening is the grinding of cutting edges: twist drills, end mills, brazed lathe tools, formers, and reamers. It is done by hand on a bench grinder for simple tools, on universal sharpening machines with cup and flat grinding wheels for end mills and drill bits, and on 5-axis CNC sharpening machines for production tools. The main rules:
- the right abrasive for the material: white corundum or CBN for high-speed steel (HSS), diamond for cemented carbide (Chapter 25);
- Use a soft grinding wheel and light passes to avoid overheating the cutting edge: a burnt cutting edge loses its hardness and won’t last long. Never cool a red-hot HSS tool in water, as it could crack; it’s better to work wet from the start;
- Where possible, the grain of the grinding wheel should run from the cutting edge toward the body, so that the burr remains on the inside and the edge does not crumble;
- The tool angles (rake angle, top rake angle, and point angle of the twist drill) are maintained by checking them with the appropriate gauges.
November 29: Polishing, Profiling, and Cooling
As it is used, the grinding wheel changes: the grains become rounded, the pores fill with chips (the wheel becomes clogged), the edge wears down unevenly, and the wheel loses its roundness and shape. Dressing removes the outer layer of the grinding wheel to restore cutting edges, open pores, and a round wheel that is coaxial with the spindle. Profiling gives the grinding wheel a specific shape (radius, angle, profile). Often, both processes are performed together using the same tool.
- a single diamond (pointed diamond) mounted on a diamond holder: it runs along the periphery of the grinding wheel, which rotates at the operating speed. It is held at a 10–15° angle in the direction of rotation and rotated around its axis from time to time to ensure even wear and keep it sharp;
- laminated and multi-grain diamonds: with more small grains in a bond, they last longer and provide a more even polish;
- diamond roller: a disc coated with diamonds that rotates under motor power and copies the entire profile onto the grinding wheel in a single pass. It is very expensive, but in mass production it can shape a complex profile in just a few seconds;
- wheeled air circulators or steel star discs and abrasive sticks for bench grinders.
As the diamond passes through the rotating grinding wheel, it leaves a very fine thread on its surface, with a pitch equal to the fd dressing feed per revolution of the wheel. It is this feed rate that determines how the grinding wheel will perform: a coarse feed rate (0.1–0.2 mm/revolution) results in an “open” and aggressive grinding wheel, which removes a lot of material and generates little heat but leaves a higher roughness; a fine feed rate (0.02–0.05 mm/revolution) results in a “closed” and smooth grinding wheel, suitable for finishing. The coverage ratio Ud is also used, which is the number of times the diamond passes over each point: the width of the diamond’s contact divided by fd.
The grinding wheel in Example 29.10 rotates at 1,671 rpm. It is dressed with a wide diamond with a contact width (bd) of 0.5 mm. How long does one pass last with fd = 0.05 mm/rev (finishing) and with fd = 0.15 mm/rev (roughing)? What is the value of Ud?
The Ø400 grinding wheel can be used up to Ø300 (below that, the flanges are no longer sufficient and the speed becomes too low). Each time the wheel is dressed, 2 passes of 0.025 mm are removed from the radius. How many dressings are performed? If 10 are done per shift, how many shifts does it take? At Ø300 and 1,671 rpm, what would the cutting speed be?
The calculation shows that most of the grinding wheel is used for dressing, not for actual grinding: dressing only as much as necessary saves on grinding wheels and time.
Refrigeration
In grinding, coolant is not optional: it removes heat, which would otherwise burn the workpiece; it lubricates the contact between the abrasive grains and the material; it cleans the pores of the grinding wheel; and it removes chips and dislodged abrasive grains. Water-in-oil emulsions (approximately 3 to 5%) are used for most grinding operations, while pure oils are used for profile, threads, and gear grinding, where finishing and profile durability are most important.
- The coolant stream must strike the contact area directly, using a shaped nozzle as wide as the grinding wheel and traveling at a speed close to that of the wheel: around a grinding wheel rotating at 35 m/s, a veil of air forms that repels the low-pressure coolant. Often, a scraper is also installed to cut through this veil;
- The coolant must be filtered thoroughly (paper filters, cartridge filters, magnetic separators): any chips or grit that re-enter the circulation would scratch the workpiece;
- The water jet must be turned on before the grinding wheel touches the workpiece and turned off afterward; with the machine stopped, let the grinding wheel spin for a few moments with the water jet turned off to spin out any liquid remaining in the pores, which would otherwise cause it to become unbalanced.
29.12 Grinding Defects and Initial Parameters
Most grinding defects stem from three causes: excessive heat, vibrations, or a dirty grinding wheel or coolant. Knowing how to recognize them can save you a lot of workpieces.
| Defect | How to Recognize It | Causes | Remedies |
|---|---|---|---|
| Burns | yellow, brown, or blue spots (reaction colors; see Chapter 22); dark or light areas when tested with an acid solution | grinding wheel too hard or clumpy, cut too deep, insufficient coolant or improperly directed, q too high | a softer, more open grinding wheel; sharpen more often and with fd bigger, lighter, more coolant, faster workpiece |
| Grinding Cuts | a network of extremely fine cracks, often invisible to the naked eye: they can be detected using magnetic particle inspection or penetrating liquids | Burn marks on hardened or case-hardened steel: the surface either re-hardens (becoming brittle) or temper, and tensile stresses develop | the same as for burn marks; proper tempering prior to grinding; no excessive allowance (paragraph 29.13) |
| Vibrations (checkerboard patterns, facets) | regular straight or helical threads with a fixed pitch, noise | unbalanced or out-of-round grinding wheel, worn bearings or belts, slender workpiece without a collet, grinding wheel that is too hard | Balance and dress the grinding wheel, use center rings, adjust the speed of the grinding wheel or the workpiece, and check the machine |
| Spiral (helix) patterns | a helical line with the longitudinal feed pitch | Unrounded edges on the grinding wheel, grinding wheel not aligned with the workpiece, feed rate too high during finishing | Slightly chamfer the edges of the grinding wheel during dressing, align the head, reduce f for finishing, and perform idle travels |
| Isolated lines and scratches | random deep scratches | grains or chips in the coolant, grinding wheel shedding grains, dirty housing | Filter the coolant, clean the machine, use a harder grinding wheel |
| Conical or oval workpiece | different diameters at both ends, or not round | misaligned table, damaged workpiece centers, workpiece heating up and expanding | Align the board, recheck the centers, cool it more thoroughly, and measure the workpiece when it's cold |
Initial Parameters
| Correction | ap roughing (mm) | ap finit. (mm) | Roughing Feed Rate | Finite feed. | vw (m/min) |
|---|---|---|---|---|---|
| Piana Beltway | 0,02-0,05 | 0,005-0,01 | 1/2–2/3 T per travel | 1/4–1/3 T per travel | 10-30 |
| Cylindrical, longitudinal pass | 0,01-0,03 | 0,002-0,005 | 2/3–3/4 T per lap | 1/4–1/2 T per lap | 15-30 |
| Cylindrical plunge cut | (radial) | (radial) | 0.002–0.005 mm/revolution | 0.0005–0.001 mm/revolution | 20-35 |
| Internal | 0,005-0,02 | 0,002-0,005 | 1/2–2/3 T per lap | 1/4–1/3 T per lap | 20-40 |
| Without through holes | 0.02–0.1 on the diameter | 0.005–0.02 on the diameter | 1–5 m/min | 0.5–2 m/min | 20-40 |
Approximate values prepared by CNC Simulator Italiafor steels using corundum-bonded grinding wheels at 30–35 m/s. Depths refer to the radius unless otherwise specified; T is the width of the grinding wheel. For hardened steels, the values tend to be on the lower side; with CBN grinding wheels and rigid machines, they increase significantly.
29.13 Grinding Allowance
The allowance is the material left on the workpiece after previous machining operations prior to grinding. It must be large enough to remove distortions caused by heat treatment, the decarburized layer, and tool marks, yet small enough to avoid wasting time and overheating the workpiece with too many passes. Chapter 22 (section 22.14) provides the formula for calculating it on the actual workpiece, based on the runout of the dial indicator after heat treatment: s = 2 · (e + amin). As an initial estimate, before the workpiece’s behavior is known, a table is used.
| Diameter (mm) | Unhardened or unquenched | Thoroughly tempered | Case-hardened and tempered |
|---|---|---|---|
| up to 10 | 0,10-0,15 | 0,15-0,20 | 0,20-0,25 |
| more than 10, up to 30 | 0,15-0,20 | 0,20-0,30 | 0,25-0,35 |
| more than 30 up to 60 | 0,20-0,25 | 0,30-0,40 | 0,35-0,45 |
| more than 60 up to 120 | 0,25-0,30 | 0,40-0,50 | 0,45-0,60 |
| more than 120, up to 250 | 0,30-0,40 | 0,50-0,60 | 0,60-0,80 |
Allowance on the diameter in mm; approximate values prepared by CNC Simulator Italia for steel shafts up to approximately 10 times the diameter in length. For slimmer shafts, the value tends toward the upper limit or exceeds it; for holes, allow a little more; for flat surfaces, 0.1 to 0.3 mm per side, depending on size and deformation. In case-hardened workpieces, the allowance is removed from the hardened layer: this must be communicated to the case-hardener (Chapter 22).
A 42CrMo4 shaft must be ground to Ø55 h6 after hardening. On identical workpieces, after straightening, a dial indicator reads 0.10 mm of runout; at least 0.08 mm must be removed from each side. What diameter is left for the lathe? Is this value consistent with the table? How much material will be removed during grinding if the diameter increases by 0.1% during heat treatment?
Using the parameters from the table in Section 29.12, this means, for example, 8 roughing passes of 0.02 mm on the radius and 4 finishing passes of 0.005 mm, plus the idle travels: the same calculation as in Example 29.10.
29.14 Lapping, Sanding, Superfinishing, and Polishing
When grinding is not sufficient—because roughness below 0.1 µm, flatness in the tenths of a micrometer range, or a nearly perfect geometric shape are required—machining operations using even finer abrasives, at low speeds and low pressure, are employed. These processes remove very little material (from a few micrometers to a few hundredths of a millimeter) and must therefore be performed on surfaces that have already been carefully ground or turned.
Lapping
In lapping, the workpiece is rubbed against a lapping surface (made of pearlitic cast iron, copper, or steel, with grooves that hold the abrasive) coated with a paste or liquid containing a dispersed abrasive: silicon carbide, corundum, boron carbide, or diamond powder, with grain sizes ranging from 40 µm down to less than 1 µm. The loose grains roll between the workpiece and the surface, removing minute particles. The workpiece moves in constantly varying paths (figure-eight, spiral) so that no point is traversed twice in the same way: in this way, the flatness of the surface is transferred to the workpiece, and the surface becomes matte with marks in all directions (symbol M, Chapter 16).
Two-disc lapping machines simultaneously machine the two parallel faces of seals, plates, valves, and injection pump parts. Stop blocks (plane-parallel blocks, Chapter 32) are the best-known example: their surfaces are lapped so flat and smooth that, when slid over one another, they stick together on their own (“adhesion”). Lapping achieves a surface roughness (Ra) of 0.05 to 0.2 µm (up to 0.025) and tolerance grades IT3–IT5.
Honing
The polishing, in English honing, is the finishing of the holes, especially engine cylinders, hydraulic cylinders, connecting rods, and rifle barrels. A head can hold two to eight abrasive stones (corundum, silicon carbide, CBN, or diamond) pressed against the wall by an expansion cone; the head turn and in the meantime goes up and down along the hole. Each grain thus traces a spiral: ascending in one direction and descending in the other. The characteristic mark remains on the wall network of intersecting grooves (Symbol X from Chapter 16).
In engine cylinders, the crossing angle is usually kept between 40° and 60°: the grooves retain the oil, and the piston ring glides over a continuous film. Plateau honing is often used: first, a coarse honing that carves deep grooves, followed by a fine honing that smooths only the ridges, leaving small, smooth “plateaus” for support and deep grooves for the oil. Grinding also corrects the shape of the hole (taper, ovality, roundness), because the long grinding wheels and the floating head follow the axis of the hole itself; it achieves a surface roughness (Ra) of 0.1 to 0.4 µm and a surface finish of IT5–IT6.
A motor cylinder with a diameter of 80 is being polished with the head rotating at 200 rpm. What axial speed is required for a crossing angle of 45°? If the travel is 150 mm, how many double travels per minute does the head make?
Superfinishing
In the superfinishing (in English superfinishing) An abrasive stone with a very fine grain, as wide as the surface, is pressed gently against the slowly rotating workpiece, and meanwhile fluctuates back and forth along the axis with short, rapid strokes (a few millimeters, from a thousand to a few thousand runouts per minute), in a light oil bath. It removes only the ridges left by grinding—ranging from 2 to 10 µm—and the surface layer damaged by heat. It is used on bearing races, crankshaft and camshaft shafts, and valve stems. It reaches Ra from 0.05 to 0.2 µm, with a profile featuring smoothed peaks that is well-suited for sliding; it does not correct large measurement errors because it removes too little material.
Polishing and Tumbling (Overview)
Polishing is done using felt, canvas, or cotton discs that spin rapidly, coated with very fine abrasive pastes: it produces a mirror-like finish for aesthetic purposes (faucets, cutlery, molds for transparent plastic), but it does not improve either the dimensions or the shape; on the contrary, it rounds off the edges. Tumbling involves placing many small workpieces in a vibrating or rotating tank along with abrasive media (ceramic, plastic, or steel) and a liquid: in a few hours, it removes burrs, rounds off edges, and standardizes the appearance of thousands of workpieces at a time, at a very low cost.
What You Get
| Machining | Normal Ra (µm) | Ra (µm) | Typical IT Job Titles | Typical removal |
|---|---|---|---|---|
| Correction | 0,2 a 1,6 | 0,05 a 3,2 | IT5-IT6 | 0.1–0.5 mm on the diameter |
| Honing | 0,1 a 0,4 | 0,025 a 0,8 | IT5-IT6 | 0.02–0.1 mm on the diameter |
| Lapping | 0,05 a 0,2 | 0,025 a 0,4 | IT3–IT5 | 0.005–0.02 mm |
| Superfinishing | 0,05 a 0,2 | 0,025 a 0,4 | the size doesn't change | 2–10 µm |
| Polishing | 0,025 a 0,1 | up to 0.012 | the size doesn't change | a few µm |
| Tumbling | based on the abrasive particles | usually not less than 0.2 | the size doesn't change | burrs and edges |
Approximate values. The Ra ranges for grinding, sanding, lapping, and superfinishing are the same as those in the table in Chapter 16 (Section 16.8); those for polishing and tumbling depend heavily on the material and the polishing compounds. The measurement of roughness is explained in Chapter 36.
29.15 The Formulas in This Chapter
| What Are You Looking For? | Formula | Units |
|---|---|---|
| Volume of grains (rule of thumb) | Vg ≈ 62 − 2 · S | % |
| Peripheral speed of the grinding wheel | vs = π · D · n / 60 000 | m/s |
| Grinding wheel revolutions | n = 60 000 · vs / (π · D) | revolutions per minute |
| Workpiece Revolutions | nw = 1000 · vw / (π · d) | revolutions per minute |
| Speed Ratio | q = 60 · vs / vw | pure number |
| Surface Grinding: Layers and Travels | i = s / ap · Nc = B / fa | numbers |
| Surface Grinding: Time | t = i · Nc · Lc / (1000 · vw) | min |
| Cylindrical Grinding: Travels and Travel Length | i = s / (2 · ap) · Lc = L − T/3 | number, mm |
| Cylindrical Grinding: Time | t = i · Lc / (f · nw) | min |
| Dive: Radial Feed and Time | vfr = fr · nw · t = x / vfr | mm/min, min |
| Specific removal | Q'w = π · d · vfr / 60 | mm³/(mm·s) |
| Centerless: axial feed | vfa = π · dr · nr · sin α | mm/min |
| Centerless: workpiece revolutions | nw ≈ nr · dr / d | revolutions per minute |
| Polishing: Speed and Time | vfd = fd · ns · td = T / vfd | mm/min, min |
| Degree of coverage | Ud = bd / fd | pure number |
| Allowance After Hardening (Chapter 22) | s = 2 · (e + amin) | mm |
| Sanding: crossing angle | tan(α/2) = va / vt · vt = π · D · n / 1000 | degrees, m/min |
29.16 Exercises
Try to solve them on your own, using a calculator, before looking at the solution.
Solution
vs = 3,1416 · 400 · 1500 / 60 000 = 31,42 m/s.
Solution
nmax = 60,000 · 50 / (3.1416 · 250) = 3,819.7 rpm: Do not exceed approximately 3,800 rpm.
Solution
n = 60,000 · 35 / (3.1416 · 500) = 1,336.9 rpm, approximately 1,337. At Ø400: vs = 3.1416 × 400 × 1,337 / 60,000 = 28.00 m/s. To return to 35 m/s, 1,671 rpm would be required.
Solution
nw = 1000 · 18 / (3.1416 · 60) = 95.5 rpm; q = 60 · 33 / 18 = 1980 / 18 = 110. Yes, it falls within the 100–125 range for external cylindrical grinding of steels.
Solution
i = 0.1 / 0.01 = 10 + 2 = 12 layers; Nc = 80 / 8 = 10 travels; Lc = 200 + 30 = 230 mm. t = 12 · 10 · 230 / (1,000 · 15) = 27,600 / 15,000 = 1.840 min = 110.4 s.
Solution
nw = 1000 · 15 / (3.1416 · 30) = 159.2 → 160 rpm; Lc = 150 − 30 / 3 = 140 mm; t = 10 · 140 / (20 · 160) = 1400 / 3200 = 0.4375 min = 26.25 s.
Solution
Radial distance x = 0.2 / 2 = 0.1 mm; t = 0.1 / 0.5 = 0.2 min = 12 s; with the shutdown, 12 + 2 = 14 s.
Solution
sin 2° = 0.03490; vfa = 3.1416 × 300 × 30 × 0.03490 = 28,274.3 × 0.03490 = 986.8 mm/min; workpieces = 986.8 / 40 = 24.7 per minute.
Solution
Grinding wheel ≈ 0.75 × 40 = 30 mm; n = 60,000 × 30 / (3.1416 × 30) = 19,099 rpm, approximately 19,100.
Solution
n = 60,000 · 35 / (3.1416 · 350) = 1,909.9 rpm; vfd = 0.1 · 1909.9 = 191.0 mm/min; td = 50 / 191.0 = 0.262 min = 15.7 s.
Solution
e = 0.06 / 2 = 0.03 mm; s = 2 · (0.03 + 0.07) = 0.20 mm: turn to Ø20.20. The table, for through-hardening between 10 and 30 mm, gives 0.20–0.30 mm: this value is at the very low end, which is correct for a short, well-straightened pin.
Solution
vt = 3.1416 × 90 × 180 / 1000 = 50.89 m/min; tan(α/2) = 15 / 50.89 = 0.2947 → α/2 = 16.42° → α = 32.8°. To reach 40°–60°, you must increase the axial speed or reduce the rotational speed.
Solution
C: silicon carbide; 46: medium grit, grains approximately 0.37 mm; J: soft hardness; 8: open structure; V: vitrified bond. This is a soft, open-structured silicon carbide grinding wheel: suitable for grinding cast iron or non-ferrous metals that tend to stick, with large contact surfaces and minimal heat generation. It is not suitable for steels.